Ti-Pd合金电化学消氢处理

Electrochemical hydrogen relief of Ti-Pd alloy
下载PDF
导出
摘要 采用电化学消氢方法对氢脆的Ti-Pd合金试样进行了消氢处理,研究了消氢电位和消氢时间对Ti-Pd合金氢含量的影响。结果表明,经过电化学消氢处理后,Ti-Pd合金的金相显微组织变得细小均匀,显微硬度降低。 Hydrogen relief treatment on hydrogen embrittlement of titanium palladium alloy was conducted by electrochemical methods. Influences of hydrogen relief potential and hydrogen relief time on the content of hydrogen were studied. Results showed that after hydrogen relief, the micro-structure of titanium palla- dium alloy became thinnet and the micro-hardness was reduced.
出处 《南京工业大学学报(自然科学版)》 CAS 北大核心 2013年第3期92-95,共4页 Journal of Nanjing Tech University(Natural Science Edition)
基金 江苏省普通高校研究生科研创新计划(CXZZ11_0328) 江苏高校优势学科建设工程资助项目
关键词 Ti-Pd合金 氢脆 电化学消氢 Ti-Pd alloy hydrogen embrittlement electrochemical hydrogen relief
  • 相关文献

参考文献5

  • 1Fekry A M. The influence of chloride and sulphate ions on the corrosion behavior on the corrosion behavior of Ti and Ti6A14V alloy in oxalic acid [ J ]. Eleetrochim Aeta, 2009,50 ( 12 ) : 3480 - 3489.
  • 2Maweja K, Phasha M J, Yamabe-Mitarai Y. Alloying and micro- structural changes in platinum-titanium milled and annealed pow- ders [ J ]. Journal of Alloys and Compounds ,2012,523 : 167 - 175.
  • 3福冢敏夫,李佐臣.钯在钛钯合金中吸氢的作用[J].稀有金属材料与工程,1982,4:75-81.
  • 4师红旗,周灿旭,丁毅,马立群.钛制换热器氢腐蚀破坏失效分析[J].腐蚀科学与防护技术,2009,21(2):137-139. 被引量:12
  • 5闫茂成,翁永基,王俭秋,柯伟.研究电化学充氢过程中X70钢氢吸收的新方法[J].材料研究学报,2007,21(4):343-347. 被引量:4

二级参考文献14

  • 1余存烨.石化钛设备腐蚀氢脆检测与安全评定[J].石油化工腐蚀与防护,1996,13(1):20-22. 被引量:5
  • 2Sergei A.Shipilov,Iain Le May,Structural integrity of aging buried pipelines having cathodic protection,Engineering Failure Analysis,13,1159(2006).
  • 3Jarmila Woodtli,Rolf Kieselbach,Damage due to hydrogen embrittlement and stress corrosion cracking,Engineering Failure Analysis,7,427(2000).
  • 4B.Gu,J.Luo,X.Mao,Hydrogen-facilitated anodic dissolution-type stress corrosion cracking of pipeline steels in near-neutral pH solution,Corrosion,55(1),96(1999).
  • 5Kumkum Banerjee,U.K.Chatterjee,Hydrogen permeation and hydrogen content under cathodic charging in HSLA 80 and HSLA 100 steels,Scripta Mater.,44,213(2001).
  • 6E.Lunarska,Y.Ososkov,Y.Jagodzinsky,Correlation between critical hydrogen concentration and hydrogen damage of pipeline steel,International Journal of Hydrogen Energy,22(2-3),279(1997).
  • 7J.Mech,Mechanics and thermodynamics on the stress and hydrogen interaction in crack tip stress corrosion:experiment and theory,Phys.Solids,46(6),1125(1998).
  • 8M.J.Danielson,Use of the Devanathan-Stachurski cell to measure hydrogen permeation in aluminum alloys,Corrosion Science,44,829(2002).
  • 9P.Manolatos,M.Jerome,C.Duret-thual,J.Le Coze.The electrochemical permeation of hydrogen in steels without palladium coating.Part Ⅰ:interpretation difficulties,Corrosion Science,37(11),1773(1995).
  • 10Y.F.Cheng,L.Yang,F.King,Analysis of hydrogen permeation through pipeline steel in near-neutral pH SCC environments,Proceedings of International Pipeline Conference,American Society of Mechanical Engineers,Calgary,Canada,2000,vol.2,1479.

共引文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部