摘要
通过对交趾黄檀与古夷苏木的FTIR分析比较,发现:交趾黄檀在1452cm-1处具有明显的C-H弯曲振动特征吸收峰,而古夷苏木在该处的吸收峰消失,该处特征吸收峰的有无可以作为区别这两种木材的波普特征之一。交趾黄檀与古夷苏木在1585/1511、1384/2922、1629/1733、1384/1733、1128/1733、1040/1733、1629/1128、1128/1040cm-1等位置的特征峰吸收强度比值存在明显的差距,也可以作为区别这两种木材的波普特征。
Through compare Dralbergia cochichinensis with Guibourtia conjugate, the FTIR spectra features to distinct them were found. First, the absorption peaks at 1452 cm^-1 that caused by C-H bending vibration was obviously in Dralbergia cochichinensis but disappeared in Guibourtia conjugate, it can be looked as a spectra feature to distinct them. Second, there are obviously difference in absorption strength ratio, such as 1585/1511, 1384/2922, 1629/1733, 1384/1733, 1128/1733, 1040/1733, 1629/1128, 1128/1040 cm^-1, which also can be looked as the spectra feature to distinct them.