以云南某辉钼矿为研究对象,通过不同捕收剂的比较,确定药剂制度,最终选用煤油为捕收剂进行闭路试验,从钼品位为0.166%原矿中,获得钼品位为55.27%、回收率为96.82%的合格钼精矿,取得了较好的选别指标。
Molybdenite ores from Yunnan were studied as the object.Through the collector comparison tests to determine the reagent regime,finally the kerosene was selected as the collector for the flotation of molybdenite minerals and closed-circuit was conducted.The concentrate grading of 55.27% Mo was obtained by the closed-circuit test with recovery of 96.82%,while the grade of run-of-mine ore was only 0.166%,and satisfactory indexes were achieved.
出处
《有色金属(选矿部分)》
CAS
北大核心
2013年第4期17-20,共4页
Nonferrous Metals(Mineral Processing Section)
关键词
辉钼矿
捕收剂
钼精矿
molybdenite
collector
molybdenum concentrate