摘要
采用高压辊磨机破碎贫赤铁矿,分别研究了辊面速度、辊面压力、矿石含水率等操作因素对中料和边料产品粒度特性的影响.结果表明:增加辊面压力,中料和边料产品粒度变细,中料产品粒度分布更加集中,边料产品粒度分布更加均匀;提升一定的辊面速度,中料产品粒度变细,粒度分布更加集中,继续提升辊面速度,中料产品粒度特性无明显变化,辊面速度变化对边料产品粒度特性影响不明显;提高给料矿石的含水率,中料和边料产品细度变化不明显,中料产品粒度分布更加集中,边料产品粒度分布更加均匀.
Low-purity hematite was crushed with high pressure grinding roll,and effects of operating factors such as roller surface pressure and speed,and ore moisture content on size of crashed products were studied.With the increase of roller surface pressure,the overall size became smaller,and size of products crushed in the roller center was distributed more concentratedly,while at the roller edge was more evenly.The products in the center became finer when the roller speed was increased into certain range,however,if further accelerating speed,no size change was observed.Roller speed had no obvious effect on the product size at edge.When the ore moisture content was increased,no obvious change was detected in product fineness.The product size distribution in the center was more concentrated,while at the edge it was more even.
出处
《东北大学学报(自然科学版)》
EI
CAS
CSCD
北大核心
2013年第8期1188-1191,1201,共5页
Journal of Northeastern University(Natural Science)
基金
中央高校基本科研业务费专项资金资助项目(N100401007)
教育部新世纪优秀人才支持计划项目(NCET-10-0308)
国家高技术研究发展计划项目(2012AA062301)
关键词
高压辊磨机
辊面压力
辊面速度
矿石含水率
贫赤铁矿
产品粒度
high pressure griding roll
roller surface pressure
roller surface speed
moisture content of the ore
low-grade hematite
product size