摘要
西钢炼钢连铸工艺改变后,第二棒材厂采用的连铸坯规格由150mm×150mm×12 000mm改为165mm×165mm×12 000mm,2012年11月初对棒材厂进行技术改造,增加轧机以适应生产工序的变化。选择好轧机机组的类型和组合形式,通过改造减轻现有主机列传动减速机的负荷,降低设备故障率,提高轧机作业率。
Specification of continuous cast bar is changed from165mm× 165mm ×12 000mm to 150mm ×150mm ×12 000mm in No. 2 line in Xilin iron and steel in October 2012 after continuous cast process reformed. In early November 2012,Bar plant began to transform to increase the mills to adapt to the changes of the new procedure, and good combination of form and type of the column of mills, were chosen in order to reduce the load of the existing host reduction gear, to reduce equipment failure rates and enhance the purpose of the mill operating rates, in order.