摘要
某铁矿山选厂尾矿中含铁约9.30%,具有一定的回收价值。为了实现资源的综合利用,试验对该尾矿样进行了选矿试验研究。采用螺旋溜槽进行预先富集,富集粗精矿经再磨后采用两段弱磁磁选,磁场强度为120 KA/m,开路试验可以获得品位63.74%,回收率10.09%的铁精矿。该工艺试验指标良好,使尾矿中的铁矿物得到了有效回收,为后续矿山技改提供了技术依据。
The iron contained in the tailings of a dressing plant of an iron mine is 9.30%, which has certain recovery value. In order to utilize the resource comprehensively, beneficiation tests were carried out. The tailings was treated first by pre - concentration with spiral chute, then the rougher concentrate was reground and went to a two - stage weak magnetic separation with a magnetic inten- sity of 20 KA/m. The open circuit test could output an iron concentrate containing 63.74% TFe with a recovery of 10.09%. The iron ore has been recovered effectively by the process, and this will provide basis for the mine's subsequent technical reform.