摘要
分析总结了葫芦岛锌厂锌浸出渣挥发窑内衬砖损坏机理及原因 ,提出了内衬砖的选用原则 ,并对普通烧结镁砖、直接结合镁铬砖、铝铬砖、镁铬铝砖等几种常用内衬砖的性能指标及实际应用情况进行了对比 。
This paper analyses and sums up damage mechanism and causes of inner lining bricks in volatilizing kiln of residue from zinc leaching in Huludao Zinc Smelter, proposes principle for selecting the inner lining bricks, gives comparison of performance and application of ordinary sintered magnesia brick, direct bond Mg Cr brick, Al Cr brick and Mg Cr Al brick that are commonly used as inner lining material and describes application of Mg Cr Al brick.[
出处
《有色冶炼》
2000年第6期20-23,共4页
Non-Ferrous Smelting
关键词
锌浸出渣
挥发窑
内衬砖
镁铬铝砖
湿法炼锌
residue from zinc leaching
volatilizing kiln
inner lining brick
Mg Cr Al brick