摘要
直径 5 .5mm线材精轧时易产生堆钢 ,从设备安装精度、操作工艺等多方面分析堆钢产生的原因 ,并采取相应的措施避免堆钢 ,从而有效地控制了堆钢的产生 ,使成材率大大提高。
Piling-up of steel frequently occurs in finishing rolling of 5.5?mm high speed wire rod.Analysis hs been made on the cause of the incident in light of the precision of equipment installation and operating process and countermeasures accordingly adopted to effectively check the incident.As the result the rate of qualified products is greatly raised.
出处
《武钢技术》
CAS
2000年第6期29-30,51,共3页
Wisco Technology