摘要
对攀钢5.5 m大容积捣固焦炉配套干熄焦干熄率提高的影响因素进行了分析,通过采取环形风道预留合理膨胀缝、牛腿结构优化、焦罐材质改进等改造措施,干熄焦率由改造前的74%提升至83%,蒸汽增产0.975万吨/月,效益显著。
This paper analyzes the factors of Panzhihua Iron and 5. 5 m high volume stamping coke oven CDQ rate increasing,A series of measures have been taken,For example reserved reasonable Expansion Joints,Corbels Structural optimization,Coke Cans material improvement,CDQ rate from transformation of the former 74% to 83%,steam production 0. 975 tons / month,efficiency significantly.
出处
《四川冶金》
CAS
2013年第3期39-43,共5页
Sichuan Metallurgy
关键词
捣固焦炉干熄焦
高径比
膨胀缝
材质优化
tamping coke oven CDQ
height to diameter ratio
expansion joints
material optimization