摘要
采用全湿法工艺浸出湿法炼锌净化镍钴渣,活化剂进行锌钴分离回收钴。结果表明,采用下述二段浸出工艺:温度70℃,反应时间1.5h,液固比4:1,一段浸出终点pH4.5~5.0,二段浸出终点pH〈0.5,锌浸出率大于98%以上,回收率95%以上。
Ni-Co-bearing purification slag from zinc hydrometallurgy was leached by full hydrometallurgy and Zi-Co was separated with activating agent to recover cobalt. The results show that the zinc leaching rate is above 98% with recovery rate of above 95% under the following optimum two-stage leaching processes including leaching temperature of 70 ℃, leaching time of 1.5 h, ratio of liquid to solid of 4: 1, pH of the end of first leaching stage of 4.5-5.0, pH of the end of second leaching stage of under 0.5.