摘要 In order to clarify the slag system of high Cr2O3 vanadium-titanium magnetite smelting in BF (blast furnace), the melting properties of slag samples prepared by analytically pure reagents were measured. By means of orthogonal test synthetic weighted score method, the optimal slag for high Cr2O3 vanadium-titanium magnetite was obtained, which contained 10% MgO, 8% TiO2 and 15% Al2O3, with the binary basicity being 1.15. In addition, the effects of basicity, MgO, TiO2 and A12 03 on slag melting properties were investigated by single factor test, and the results showed that, with increasing the basicity or TiO2 content, melting temperature (Tin) increased, whereas initial vis- cosity (r/0) and high temperature viscosity (r/h) decreased. With increasing the MgO content, Tm decreased firstly and then increased. With increasing the Al2 O3 content, Tm increased, and η0 and r/h decreased firstly and then increased. In order to clarify the slag system of high Cr2O3 vanadium-titanium magnetite smelting in BF (blast furnace), the melting properties of slag samples prepared by analytically pure reagents were measured. By means of orthogonal test synthetic weighted score method, the optimal slag for high Cr2O3 vanadium-titanium magnetite was obtained, which contained 10% MgO, 8% TiO2 and 15% Al2O3, with the binary basicity being 1.15. In addition, the effects of basicity, MgO, TiO2 and A12 03 on slag melting properties were investigated by single factor test, and the results showed that, with increasing the basicity or TiO2 content, melting temperature (Tin) increased, whereas initial vis- cosity (r/0) and high temperature viscosity (r/h) decreased. With increasing the MgO content, Tm decreased firstly and then increased. With increasing the Al2 O3 content, Tm increased, and η0 and r/h decreased firstly and then increased.
出处 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2014年第2期144-150,共7页 钢铁研究学报(英文版)
基金 Item Sponsored by National Natural Science Foundation of China(51090384) National High Technology Research and Development Program(863 Program)of China(2012AA062302,2012AA062304) Fundamental Research Funds for the Central Universities of China(N110202001)
关键词 high Cr2 03 vanadium-titanium magnetite melting property slag optimization synthetic weighted scoremethod high Cr2 03 vanadium-titanium magnetite melting property slag optimization synthetic weighted scoremethod
  • 相关文献

参考文献20

  • 1S.Y.Gou.查看详情[J],Iron Steel Vanadium Titanium2009(3):8-9.
  • 2J.Y.Ma.Theory and Practice for Vanadium Titanomagnetite in Blast-furnace Process[M]{H}北京:冶金工业出版社,2000.
  • 3S.A.Krasikov;L.A.Maiorov;A.A.Ponomarenko;S.V.Zhidovinova A.A.Sawinona.查看详情[J],{H}STEEL IN TRANSLATION2011752-755.
  • 4Y.Zhou;W.C.Jiang;B.S.Wang.查看详情[J],J Iron Steel Res1985(4):445-450.
  • 5B.Jia;B.M.Qi.查看详情[J],Iron Steel Vanadium Titanium1996(4):10-14.
  • 6Y.L.Su;L.J.Wu;C.Y.Song.查看详情[J],Iron Steel Vanadium Titanium2002(3):9-16.
  • 7M.Y.Zhu.Metallurgy of Iron and Steel[M]{H}北京:冶金工业出版社,2008.
  • 8P.G.Mo;J.S.Chen.查看详情[J],Acta Metall Sin1964(7):363-374.
  • 9J.C.Tao;J.M.Wu.查看详情[J],Systems Engineering Theory & Parctice2001(8):43-48.
  • 10Orthogonal Test Group in Department of Mathematics Peking University. Method of Orthogonal Test[M].Scientific Popularization Press,Beijing,1979.

同被引文献40

  • 1李福民,吕庆,胡宾生,于勇,陶文.高炉渣的冶金性能及造渣制度[J].钢铁,2006,41(4):19-22. 被引量:41
  • 2朱苗勇.钢铁冶金学[M].北京:冶金工业出版社,2005:75-77.
  • 3Sadykhov G B, Karyazin I A. Titanium-vanadium slags produced upon the direct reduction of iron from titanomagnetite concentrates [ J ]. Russian Metallurgy (MetaUy) ,2007,2007 ( 6 ) :447 - 454.
  • 4Logachev G N, Gostenin V A, Pishnograev S N, et al. Mobility of blast-furnace slag [ J ]. Steel in Translation, 2013,43(12) :805 -807.
  • 5Shankar A, Gomerup M, Lahiri A K, et al. Experimental investigation of the viscosities in CaO-SiO2-MgO-A1203 and CaO-SiO2-MgO-A1203-TiO2 slags[ J ]. Metallurgical and Materials Transactions B,2007,38 ( 6 ) :911 - 915.
  • 6Jan Y C, Hae G L, Jeong S K. Dissolution rate of A12 O3 into molten CaO-SiO2-AI203 slags [ J]. ISIJ International,2002, 42(8) :852 -860.
  • 7Zhang G H, Chou K C, Mills K. Modelling viscosities of CaO-MgO-A1203-SiO2 molten slags [ J]. ISIJ International, 2012,52(3) :355 -362.
  • 8SADYKHOV G B, KARYAZIN I A. Titanium-vanadium slags produced upon the direct reduction of iron from titanomagnetite concentrates[J]. Russian Metallurgy (Metally), 2007, 2007(6): 447-454.
  • 9GAO Yanhong, BIAN Lingtao, LIANG Zhongyu. Influence of B203 and TiO2 on viscosity of titanium-beating blast furnace slag[J]. Steel Research International, 2014, 86(4): 386-390.
  • 10DONG Xiangjuan, SUN Haoyan, SHE Xuefeng, et al. Viscosity and viscosity estimation model of fully liquid slags in TiO2-A1203-CaO-SiO2 and TiO2-AI203-CaO-SiO2-MgO systems with high TiO2 concentration and low mass ratio of CaO to SiO2[J]. Ironmaking and Steelmaking, 2014, 41(2): 99-106.

引证文献5

二级引证文献24

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部