镍钼矿尾矿表面改性-浮选研究 被引量:1

Surface Modification and Flotation of Tailings from Ni-Mo Separation
下载PDF
导出
摘要 针对某镍钼矿尾矿,通过表面改性条件试验、改性尾矿的开、闭路浮选试验探索,设计出合理的加工流程。在磨矿粒度-0.074 mm粒级占90%,改性剂石灰用量为2 500 g/t,改性作用时间为45 min,改性浓度60%,搅拌速度700 r/min的条件下,获得了可选性最好的改性尾矿。在闭路浮选流程下,可以获得Mo品位为3.82%,回收率41.26%的精矿,同时精矿含有8.56%的Ni。 Based on the studies on surface modification measures /or N1-Mo ilotation talllngs, open ana closecl-clrcmt flotation tests of modified tailings were carried out, and a rational processing flowsheet was accordingly proposed. Modified tailings with the best separability can be prepared with a grinding fineness of 90% -0.074 mm, lime dosage of 2 500 g,(t, reaction time of 45 min, concentration of 60% and agitation speed of 700 r/min. For the closed-circuit test, a concentrate with Mo grade and recovery of 3.82% and 41.26%, respectively, can be obtained, while the Ni content therein is 8.55%.
出处 《矿冶工程》 CAS CSCD 北大核心 2014年第1期37-40,43,共5页 Mining and Metallurgical Engineering
基金 国家高技术研究发展计划("863"计划)项目(2007AA06Z129)
关键词 镍钼矿 尾矿 表面改性 浮选 分子动力学模拟 Ni-Mo ore tailings surface modification flotation molecular dynamics simulation
  • 相关文献

参考文献17

  • 1袁明亮,李俊,胡岳华.复杂铝土矿浮选尾矿机械力化学表面改性研究[J].矿产综合利用,2005(2):3-7. 被引量:8
  • 2HU Xi-xue, Shen Hong, Chen Yan, et al. One-step modification of nano-hydroxyapatite coating on titanium surface by hydrothermal meth- od [J].Surface & Coatings Technology, 2010, 205 : 2000-2006.
  • 3蔡春林,覃文庆,邱冠周,徐本军.表面改性对JT-235浮选铜钼矿的影响[J].湿法冶金,2006,25(4):205-207. 被引量:1
  • 4May F, Cock E, Vogt V, et al. Plasma-modification of sulfides for optimizing froth-flotation properties [ J ]. Minerals Engineering, 2012, 35 : 67- 74.
  • 5Govender S, Swart P. Surfactant formulations for multifunctional sur- face modification [ J ]. Colloids and surfaces A : Physicochemical and Engineering Aspects, 2008,331:97-102.
  • 6WANG Ming-yu, WANG Xue-wen, LIU Wan-li. A novel technology of molybdenum extraction from low grade Ni-Mo ore[ J ] .Hydmmetal- lurgy, 2009,97 : 126-130.
  • 7CHEN Jia-wu, GAO Cong-jie, ZHANG Qi-xiu. Leaching of nickel- molybdenum ore in membrane biological reactor [ J ]. Transaction of Nonferrous Metals Society of China, 2011,21 : 1395-1401.
  • 8X Ye, S Gredeli, W Skinner, et al. Evidence for surface cleaning of sulphide minerals by attritianing in stirred mills [ J ]. Minerals Engi- neering, 2010,23(11-13) :937-944.
  • 9DING Hao, Lu Shou-ci, DU Gao-xiang. Surface modification of wol- lastonite by the mechano-activated method and its properties [ J ]. In- ternational Joumals of Minerals Metallurgy and materials, 2011,18 (1) :83.
  • 10段希祥.碎矿与磨矿[M].北京:冶金工业出版社,2006.

二级参考文献34

共引文献90

同被引文献14

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部