摘要 为给丹寨县某硫化铅锌矿石的开发利用提供技术依据,在对矿石进行工艺矿物学研究基础上,采用优先浮铅再浮锌流程进行了铅锌选矿试验。结果表明,在磨矿细度为-0.074 mm占80%,铅粗选CaO用量为2 500 g/t、ZnSO4+Na2SO3为1 500+1 000 g/t、乙硫氮+丁铵黑药为10+10 g/t、2#油为18 g/t,锌粗选CuSO4用量为600 g/t、丁基黄药用量为130 g/t情况下,采用1粗1精1扫浮铅、1粗1精2扫浮锌、中矿顺序返回流程处理该矿石,获得了铅品位为48.72%、含锌4.95%、铅回收率为89.21%的铅精矿,以及锌品位为45.89%、含铅0.72%、锌回收率为82.42%的锌精矿。 In order to provide technical basis for development and utilization of a sulfide lead-zinc ore from Danzhai county, selective flotation tests of lead floating first and then zinc were conducted based on the process mineralogy of the ore. The results showed that,lead concentrate with Pb grade and recovery of 48.72% and 89.21% respectively, containing 4.95% zinc,and zinc concentrate with Zn grade and recovery of 45.89% and 82.42% respectively,containing 0.72% lead,were a- chieved at the grinding fineness of 80% passing - 0.074 mm, and CaO, Na2 S03 + ZnS04, ethyl thioearbamate + ammonium butylaerofloat and 2# oil dosage of 2 500 g/t, 1 500 + 1 000 g/t, 10 + 10 g/t and 18 g/t respectively for lead rough flotation, CuS04 and butyl xanthate dosage of 600 g/t and 130 g/t respectively for zinc rough flotation, by process of one-stage roughing, one-stage cleaning and one-stage scavenging for lead flotation, one-stage roughing, one-stage cleaning and two-stage scavenging for zinc flotation, and middles back to the flow-sheet in turn.
出处 《金属矿山》 CAS 北大核心 2014年第3期84-87,共4页 Metal Mine
关键词 硫化铅锌矿 抑锌浮铅 优先浮选 Sulfide lead-zinc ore, Lead flotation and zinc suppression, Selective flotation
  • 相关文献

参考文献10

二级参考文献34

共引文献153

同被引文献83

引证文献6

二级引证文献45

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部