摘要 金精矿浸出尾渣中金品位为3.61 g/t,其中93.74%被铁、硫、石英微细包裹,难以回收,采用低温常压硝酸预氧化处理后再氧化炭浸工艺,原渣品位从3.61 g/t降为1.08 g/t,金浸出率70.25%。 The gold grade of the gold concentrate leaching tailings is 3.61 g/t, and about 93.74% of the gold minerals was micro wrapped by iron, sulphur and quartz, so it is difficult to be recycled. Pre- oxidation treatment was used by nitric acid under low temperature and normal pressure, then carbonate leaching process was adopted. Finally the grade of tailings decreased from 3.61 g/t to 1.08 g/t, with leaching rate of 70.25%
出处 《有色金属(选矿部分)》 CAS 北大核心 2014年第2期49-51,共3页 Nonferrous Metals(Mineral Processing Section)
关键词 微细包裹 预处理 回收率 micro wrapped pre-treatment recovery