武钢5号高炉近年来炉身反复黏结,主要原因是锌负荷高(达1515g/t)。通过锌平衡分析,提出了降低锌富集的方法。
It is expounded in the paper that the skull occurred frequently at WISCO's No. 5 BF stack in the past few years is mainly resulted from high zinc load (up to 1515g/t) and put forwards the procedures of reducing zinc enrichment by analy- zing zinc balance.