摘要 瓦斯抽放管道性能的好坏直接关系到瓦斯抽放过程的安全与可靠,影响到煤矿井下的安全生产,一旦发生静电火花、受冲击破坏、吸瘪等情况,就可能产生非常严重的后果。对瓦斯抽放管的抗落锤冲击、耐老化、耐负压、环刚度等性能进行了试验研究,起草了煤矿用非金属瓦斯输送管材的安全生产行业技术标准。 The performance of gas drainage pipes is directly related to the safety and reliability of gas drainage process and has the influence on the safe production of coal mines. In the event of electrostatic spark, impact damage and shrinkage, they may have very serious consequences. For this purpose, test study was carried out on the performance of the gas pipes, including the hammer shock resistance, ageing resistance, negative-pressure resistance, ring stiffness and so on, and the industry technical standard for safe production in coal mines - "Safety Technical Requirements of Non-metal Gas Drainage Pipes for Coal Mine"has been drafted.
作者 孔令刚
出处 《矿业安全与环保》 北大核心 2014年第2期67-69,72,共4页 Mining Safety & Environmental Protection
关键词 非金属瓦斯输送管 安全性能 抗落锤冲击 耐老化 耐负压 环刚度 技术标准 non-metal gas delivery pipe safety performance drop hammer impact resistance aging resistance negative-pressure resistance ring stiffness technical standard
  • 相关文献

参考文献9

  • 1MT558.1-2005,煤矿井下用塑料管材第1部分聚乙烯管材[S].
  • 2MT558.2-2005,煤矿井下用塑料管材第2部分聚氯乙烯管材[S].
  • 3MT558.3-2005,煤矿井下用塑料管材第3部分玻璃钢管材[S].
  • 4MT181-88,煤矿井下用塑料管安全性能检验规范[S].
  • 5HG/T3049-1999,橡胶或塑料涂覆织物加速老化试验[S].
  • 6李少辉,孙健,王范树,邓鹏,杨华运.非金属管耐负压性能检测系统的研究[J].矿业安全与环保,2008,35(B12):11-13. 被引量:3
  • 7李跃军,于双海.井下固定式抽放瓦斯泵站设计及实施探究[J].华北科技学院学报,2006,3(1):32-34. 被引量:3
  • 8赵启辉,凌伟.热塑性塑料管材环刚度的测定GB/T9647-2003[S].中国轻工业联合会,2003.
  • 9AQ1071-2009,煤矿用非金属瓦斯输送管材安全技术要求[S].

二级参考文献3

共引文献7

同被引文献20

引证文献3

二级引证文献10

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部