摘要
以CRH2C型动车组五级修外风挡为例,主要介绍外风挡端部开裂及表面龟裂的修复工艺。
This paper mainly introduced the repair process of breaks at exterior gangway bellow ends and cracks on surface by demonstrating Level 5 maintenance practices of CRH2C High-speed EMU.
出处
《机械工程师》
2014年第4期272-273,共2页
Mechanical Engineer
关键词
动车组
外风挡
龟裂
EMU
Exterior Gangway Bellow
Crack