本文通过对首钢第二炼钢厂120mm×120mm铸机高效改造后的铜管使用情况进行调研,找出了铜管内在的磨损规律及更趋于合理的铜管锥度设计曲线。
The inherent wearing law of copper tube and the more reasonable design curve of copper tube was gained in the paper, through investigating the copper tube wearing condition after modification of continuous 120mm×120mm square caster at No.2 Steel Plant of Shougang Co..
出处
《连铸》
2001年第1期11-14,共4页
Continuous Casting