摘要
对江西某白钨矿采用优先选硫—白钨粗选—白钨粗精矿加温精选的流程,获得钨精矿WO3品位61.79%、WO3回收率74.30%的较好指标。为开发利用该类型低品位钨矿石提供了技术依据。
cleaning by warming was carried out on a scheelite ore of Jiangxi, and the concentrate grade containing 61.79% WO3 was obtained with recovery of 74.30% by the flotation test, so satisfactory result was achieved. These studies could provide technical reference for the development of these kind of low grade scheelite ore.
出处
《有色金属(选矿部分)》
CAS
北大核心
2014年第3期33-36,共4页
Nonferrous Metals(Mineral Processing Section)
基金
"十二五"国家科技支撑计划项目(2012BAB10B03)
关键词
白钨矿
浮选
加温精选
scheelite
flotation
cleaning by warming