Bimetallic Fe-Co/GAC (granular activated carbon) was prepared and used as heterogeneous catalyst in the ultrasound enhanced heterogeneous activation of peroxydisulfate (PS, S2O8 2-) process. The effect of initial pH, PS concentration, catalyst addition and stirring rate on the decolorization of Acid Orange 7 (AO7) was investigated. The results showed that the decolorization efficiency increased with an increase in PS concentration from 0.3 to 0.5 g/L and an increase in catalyst amount from 0.5 to 0.8 g/L. But further increase in PS concentration and catalyst addition would result in an unpronounced increase in decolorization efficiency. In the range of 300 to 900 r/min, stirring rate had little effect on AO7 decolorization. The catalyst stability was evaluated by measuring decolorization efficiency for four successive cycles.
Bimetallic Fe-Co/GAC (granular activated carbon) was prepared and used as heterogeneous catalyst in the ultrasound enhanced heterogeneous activation of peroxydisulfate (PS, S2O8 2-) process. The effect of initial pH, PS concentration, catalyst addition and stirring rate on the decolorization of Acid Orange 7 (AO7) was investigated. The results showed that the decolorization efficiency increased with an increase in PS concentration from 0.3 to 0.5 g/L and an increase in catalyst amount from 0.5 to 0.8 g/L. But further increase in PS concentration and catalyst addition would result in an unpronounced increase in decolorization efficiency. In the range of 300 to 900 r/min, stirring rate had little effect on AO7 decolorization. The catalyst stability was evaluated by measuring decolorization efficiency for four successive cycles.
基金
supported by the National Natural Science Foundation of China (No. 20977069, 21211130108)
the Natural Science Foundation of Hubei Province, China through "The Outstanding Youth Scholars Program" (No. 2007ABB028)