摘要
对掺加粉煤灰和矿粉后混凝土性能进行了试验研究,结果表明:28d后所有掺加矿物掺合料的混凝土强度都已超过基准混凝土强度,7、60d时,单掺35%粉煤灰强度最大,28d时单掺35%矿粉效果最佳;各矿物掺合料均能改善混凝土各龄期的抗氯离子渗透性能,且掺量越高,抗渗性能越强,养护7d时单掺50%矿粉效果最佳,而单掺50%粉煤灰对28、60d时抗渗性能的改善最为明显;复掺粉煤灰和矿粉并没有较单掺显现出明显的优势。
The performances of concrete mixed with fly ash and slag were studied ,and results showed that:after 28 d the strength of all concrete mixed with mineral admixture have exceeded the strength of reference concrete.At 7 d and 60 d ,the strength of concrete mixed with 35%fly ash is the highest.At 28 d,mixing with 35%slag,the effect is the best;all mineral admixtures can improve the anti-chlo-ride-permeability performances of concrete in every age.And the content of admixture is higher ,the anti-permeability performance is more stronger.At 7 d,the effect with 50%slag is best,but at 28 d and 60 d the anti-permeability performances improved significantly when the proportion of fly ash is 50%;The double-doped of fly ash and slag showed no obvious advantage than doped of fly ash or slag only.
出处
《混凝土》
CAS
CSCD
北大核心
2014年第6期75-77,共3页
Concrete
基金
国家自然科学基金项目(51074166
51104128)
江苏省产学研前瞻性联合研究项目(BY2012085)
住房和城乡建设部科学技术项目(2013-K4-22)
江苏省高校自然科学研究项目(11KJD130002)
徐州市科技计划项目(XZZD1320)
国家建筑材料行业科技创新计划--面上研究项目(2013-M5-7)
江苏省"青蓝工程"项目
关键词
粉煤灰
矿粉
混凝土
抗压强度
渗透性能
fly ash
slag
concrete
compressive strength
permeability