利用某铁厂低活性水淬矿渣 ,使用填加复合活性激发剂的方法在不进行煅烧的情况下 ,配制出用渣量达 80 %以上、技术指标达到 52 5R型矿渣水泥标准的环保型节能水泥 .通过测定水化热。
The experiment was carried out to make environment protecting energy saving cement without baking by using blast furnace water hardened slag of an Iron Factory. Under the condition of the propotion of slag in mixture over 80%,and the slag active agent being added in, the 525R cement can be produced. Based on the research of hydration heat and pH value and XRD patterns, the author probed into the hydnate mechanism of the cement.