期刊文献+

基于SENT试样获取材料断裂韧度的载荷分离法研究 被引量:7

Study on the Load Separation Method of SENT Specimens for Fracture Toughness Assessment
下载PDF
导出
摘要 单边裂纹拉伸(Single edged notched tension,SENT)试样因其低约束特性逐渐被用于管道材料的断裂韧度评定。根据有限元法,提出SENT试样的应力强度因子表达式,J积分计算中的增量塑性功算式以及塑性因子算式,并与文献中公式进行对比证实公式的精确性和有效性。依据ASTM用于CT试样获取断裂韧度载荷分离理论规则化方法提出适用于SENT试样的量纲一载荷分离法,并通过有限元计算证实SENT试样载荷分离的成立性。由量纲一载荷分离理论中的规则化方法完成了汽轮机低压转子材料30Cr2Ni4MoV、电站用P92管道钢以及5083-H112铝合金SENT试样断裂韧度值以及J阻力曲线测定,获得了各材料合理的J阻力曲线及条件断裂韧度JQ值。 In view of low constraint properties,single edged notched tension(SENT) specimens are gradually applied for the assessment on fracture toughness of pipe materials.Detailed analyses for the stress intensity factor,incremental plastic work and plastic factor used in the J-integral computation are conducted.The precision and validity are confirmed through the comparison between formulas obtained and references.Systematic investigation on the estimation of J resistance curves for SENT specimens is carried out on the basis of normalization method which concludes in the non-dimensional load separation method.The establishment of the load separation for SENT specimen is verified by finite element analysis.30Cr2Ni4MoV used for steam turbine low pressure rotors,T92 pipe steel and 5083-H112 aluminum alloy are employed to experimentally complete the estimation of J resistance curves of SENT specimens by using the normalization method of non-dimensional load separation and reasonable fracture toughness values are acquired.
出处 《机械工程学报》 EI CAS CSCD 北大核心 2014年第10期48-57,共10页 Journal of Mechanical Engineering
基金 国家自然科学基金资助项目(11072205)
关键词 断裂韧度 J阻力曲线 单边裂纹拉伸试样 量纲一载荷分离 规则化法 fracture toughness J resistance curves single edged notched tension(SENT) specimen non-dimensional load separation normalization method
  • 相关文献

参考文献21

  • 1CHIESA M, NYHUS B, SKALLERUD B, et al. Efficient fracture assessment of pipelines. A constraint-corrected SENT specimen approach[J]. Engineering Fracture Mechanics, 2001, 68(5): 527-547.
  • 2CRAVERO S, RUGGIERI C. Correlation of fracture behavior in high pressure pipelines with axial flaws using constraint designed test specimens- Part I: Plane-strain analyses[J]. Engineering Fracture Mechanics, 2005, 72(9): 1344-1360.
  • 3W,STBERG S, PISARSKE H, NYHUS B. Guidelines for engineering critical assessments for pipeline installation methods introducing cyclic plastic strain[C]//Proceedings of 23rd International Conference on Offshore Mechanics and Arctic Engineering, Vancouver, British Columbia, Canada, June 20-25, 2004, NewYork: ASME, 2004: 1-8.
  • 4NYHUS B, OSTBY E, KNAGENHJELM H O, et al. Experimental studies on the effect of crack depth and asymmetric geometries on the ductile tearing resistance[C]//Proceedings of 23rd International Conference on Offshore Mechanics and Arctic Engineering, June 12-17, 2005, Halkidike, New York: ASME, 2004: 1-10.
  • 5Det Norske Veritas(DNV). DNV-RP-F108 Fracture control for pipeline installation methods introducing cyclic plastic strain[M]. HOvik: Det Norske Veritas, 2006.
  • 6SHEN G, BOUCHARD R, GIANETTO J A, et al. Fracture toughness evaluation of high-strength steel pipe[C]//PVP2008-61100, Proc. ASME PVP 2008 Pressure Vessel and Piping Division Conference, July 27-3 1, 2008, Chicago: Illinois, 2008.
  • 7SHEN G, TYSON W R. Crack size evaluation using unloading compliance in single-specimen single-edge-notched tension fracture toughness testing[J]. Journal of Testing and Evaluation, 2009, 37(4): 347-357.
  • 8SHEN G, GIANETTO J A, TYSON W R. Measurement of J-R curves using single specimen technique on clamped SE(T) specimens[C/CD]//Proceedings of 18th International Conference on Offshore and Polar Engineering, June 21-26, 2009, Osaka, Japan, 2009.
  • 9SHEN G, TYSON W R. Evaluation of CTOD fromJ-integral for SE(T) specimens [C/CD]//Pipeline Technology Conference, October 12-14, 2009, Ostend, Belgium, 2009.
  • 10CRAVERO S, RUGGIERI C. Estimation procedure of J-resistance curves for SE(T) fracture specimens using unloading compliance[J]. Engineering Fracture Mechanics, 2007, 74: 2735-2757.

共引文献19

同被引文献47

  • 1刘鹏飞,陶伟明,郭乙木.中心裂纹板塑性功因子的计算[J].浙江大学学报(工学版),2004,38(8):1082-1085. 被引量:3
  • 2罗金恒,赵新伟,李新华,郑茂盛,朱杰武.X80管线钢断裂韧性研究[J].压力容器,2007,24(8):6-9. 被引量:12
  • 3李鹤林,李霄,吉玲康,陈宏达.油气管道基于应变的设计及抗大变形管线钢的开发与应用[J].焊管,2007,30(5):5-11. 被引量:108
  • 4田泽,孙学伟.确定材料J积分塑性因子η_(pl)的单试件法研究[J].实验力学,1997,12(3):475-480. 被引量:3
  • 5BEGLEY J A, LANDES J D. Fracture toughness[J]. ASTMSTP, 1972, 514: 1-20.
  • 6ZHU X K, LAMP S, CHAO Y J. Application of normalization method to fracture resistance testing for storage tank A285 carbon steel[J]. International Journal of Pressure VesselsandPiping, 2009, 86(10): 669-676.
  • 7CASSANELLI A N, ORTIZ H, WAINSTEIN J E, et al. ASTM STP 1406, separability property and load normalization in AA 6061-T6 Aluminum alloy[J]. ASTM Special Technical Publication, 2002, 1406: 49-74.
  • 8BALDI F, RICC0 T. High-rate J-testing of toughened polyamide 6/6: Applicability of the load separation criterion and the normalization method[J]. Engineering Fracture Mechanics, 2005, 72(14): 2218-2231.
  • 9American Society for Testing and Materials. ASTM E1820-11. Standard test methods for measurement of fracture toughness[S]. Philadelphia: ASTM, 2011.
  • 10中华人民共和国国家质量监督检验检疫总局,中国国家标准化管理委员会.GB/T21143-2007金属材料准静态断裂韧度的统一试验方法[S].北京:中国标准出版社,2008.

引证文献7

二级引证文献15

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部