用溶胶-凝胶低温合成方法制备了SiO2单组分凝胶纤维,纤维长大于1米。用旋转粘度计研究了溶胶-凝胶的转变过程,讨论了制备过程中各种条件对溶胶可纺性的影响,结果表明,较适宜的凝胶纤维制备TEOS:H2O:HCL:C2H5OH=1:1.7:0.01:1(mol)
:Silicon dioxide gel fiberwhich length is over one metercan be prepared with cryochemical method.The paper research the col-gel transformation and influence of condition upon sol drawability during preparotion with stiring viscosimeter. In resultthe fit ratio of gel fiber preparation is TEOS:H2O:HCL:C2H5OH=1:1.7:0.01:1(mole ratio).
出处
《山东建材》
2001年第1期8-9,3,共3页
Shandong Building Materials
关键词
凝胶纤维
可纺性
二氧化硅
制备
:gel fiber;drawability;transformationquid concret