现场试验的结果表明 ,F1/ F2混剂处理的橡胶木圆盘、单板的防霉及防蓝变效果较 F2及五氯酚钠要好。 F1/F2及五氯酚钠各制剂处理的板材基本上无霉菌感染及蓝变。在真空加压试验中 ,0 .0 2 % F2可保持橡胶木板材在气干过程中 12天基本不霉变及蓝变 ,但对白霉的防治效果较差 ;0 .0 0 94% F1与 0 .0 18% F2混合剂可保持橡胶木板材气干时 15天不长霉或蓝变 ,增加 F1/ F2的浓度可能会在气干时保持更长的时间。
The mixture formulation of chlorothalonil emulsion (F1) and mixture of chlorothalonil emulsion and other fungicide (F2) was more effective than F2 or sodium pentachlorophenol (NaPCP) alone in controlling stain and mold of rubberwood ( Hevea brasiliensis ). In pilot test, the sawntimber treated with each formulation of F1/F2 and NaPCP was not infected with stain and mold. In vacuum pressure treatment test, the result indicated that F2 could prevent the treated timber for 12 days from stain and mold except white mold; and the mixture of 0.0094% F1 and 0.018% F2 could keep the treated timber for 15 days from stain and mold in air drying procedure under the above concentrations. The higher concentrations of F1/F2 might prevent the treated timber for longer time from stain and mold.
出处
《木材工业》
2001年第2期17-19,共3页
China Wood Industry
基金
ITTO PD3/96 Rev.2(I)项目部分研究内容