摘要 以 Na BH4 为还原剂对含有二氮杂萘酮结构的聚芳醚砜酮 ( PPESK)进行羟基化改性 ,并用 FT-IR和 1H-NMR对还原后的聚芳醚砜酮 ( PPESK— OH)的结构进行表征 .通过测定玻璃化转变温度 ( Tg)、水接触角和溶解性 ,研究还原后聚合物的性能变化 .结果表明 ,随还原程度加深 ,PPESK— OH的 Tg逐渐升高 ,由 52 9.6K升至 571 .3 K,耐热性能有所改善 ;亲水性能增强 ,当还原率为 54.8%时 PPESK— OH的水接触角为 52 .6°; Poly(phthalazinone ether sulfone ketone) (PPESK) containing the phthalazinone moiety copolymer can be hydroxylated with NaBH 4 in DMAc. The reductive PPESK(PPESK—OH) is fully characterized by FT IR and 1H NMR.The properties of PPESK—OH are shown with the measuring inherent viscosity, contact angle (water), glass transition temperature ( T g ) and solubility in different solvents. The results indicate that the presence of the hydroxyl group significantly enhances the PPESK—OH film wettability; and its T g becomes higher than PPESK′s, which gives it good thermal stability. Nevertheless, the solubility of PPESK—OH has also been changed. It can be soluble in DMAc, NMP, DMF and m cresol, not soluble in chloroform, NB, TCE solvent.
出处 《大连理工大学学报》 EI CAS CSCD 北大核心 2001年第2期152-154,共3页 Journal of Dalian University of Technology
关键词 羟基化 改性 聚芳醚砚酮 二氮杂萘酮 玻璃化转变温度 溶解性 hydroxylation modification/poly(phthalazinone ether sulfone ketone)s
  • 相关文献

参考文献5

  • 1刘彦军.耐高温高性能热塑性特种工程塑料含氮杂环聚芳醚酮系列聚合物的制备和结构与性能的研究[M].大连:大连理工大学,1997..
  • 2姚蒙正 程侣柏 等.精细化工产品合成原理[M].北京:中国石化出版社,1983..
  • 3刘彦军,学位论文,1997年
  • 4NOISET O,Macromolecules,1997年,30卷,540页
  • 5姚蒙正,精细化工产品合成原理,1983年

共引文献1

同被引文献5

引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部