锅炉蒸发受热面管环向裂纹分析及处理 被引量:1

Analysis and Handling of Circular Cracks on the Evaporative Heating Surface Tubes of Boiler
下载PDF
导出
摘要 介绍1台1 021 t/h锅炉蒸发受热面水冷壁管环向裂纹失效情况,对其出现的原因从材料、水质、燃烧3方面分析认为 因水质问题引起的蒸发受热面结垢与火焰贴壁是产生裂纹的主要原因,根据燃烧理论和热力学原理阐述裂纹形成机理,并提出处理对策。 The paper briefs the circular crack failure on the water wall tubes in evaporative heating surface zone of one 1 021 t/h boiler analyzes the occurring causes in terms of material water quality and combustion holds that the scale on the evaporative heating surface arising from water quality and the flame rubbing against water wall tubes are the main causes for cracks and finally based upon the combustion theory and thermodynamics principles explains the crack-forming mechanism and puts forward the handling countermeasures.
作者 刘建国
机构地区 湖南省石门电厂
出处 《中国电力》 CSCD 北大核心 2001年第5期10-12,共3页 Electric Power
关键词 锅炉 水冷壁管 蒸发 受热面 环向裂纹 火力发电厂 water wall tubes scale flame rubbing against water wall cracks
  • 相关文献

参考文献4

  • 1杨世铭.传热学[M].高等教育出版社,1987,10..
  • 2陈学俊 陈听宽.锅炉原理(上下册)[M].北京:机械工业出版社,1983..
  • 3南京工学院 西安交通大学.电厂锅炉原理[M].北京:电力工业出版社,1982..
  • 4-.湖南省电力系统技术监督资料汇编[M].湖南省电力试验研究所,1993..

共引文献116

同被引文献50

引证文献1

二级引证文献14

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部