摘要 研究了多级喷雾碳化法制备纳米碳酸钙的工艺 ,并详细讨论了雾化、碳化条件及添加剂量等对纳米碳酸钙粒径的影响。碳化后的沉淀物经真空干燥 ,其原始粒径约为 3 0nm。经表面改性处理 ,可得到粒径在 3 0~ 40nm范围的活性纳米碳酸钙粉体材料。 In this paper,the preparation process of nanometer calcium carbonate (CaCO 3)by multistage spray carbonation was studied.The effects of the conditions of spray carbonation and additive dosage on the average particle size of nanometer CaCO 3 were discussed systematically.The primary particle size of carbonated sediment was about 30nm by vacuum desiccation.Then the active nanometer CaCO 3 particles ranged from 30nm to 40nm could be obtained with surface modification.
出处 《化工矿物与加工》 CAS 北大核心 2001年第6期5-7,24,共4页 Industrial Minerals & Processing
关键词 纳米碳酸钙 喷雾碳化法 粒径 传质系数 添加剂 表面改性处理 nanometer calcium carbonate multistage spray carbonation particle size mass transfer coefficient
  • 相关文献

参考文献1

  • 1K.马斯托思 黄照柏等(译).喷雾干燥手册[M].北京:中国建筑工业出版社,1983.156-157,160-162,555-558.

同被引文献134

引证文献10

二级引证文献52

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部