加入Ni-Al,W-Ni,W-Co二元添加剂时的CuCr25合金的组织与性能 被引量:9

Microstructures and Properties of CuCr25 Alloys Melted by Vacuum Induction
下载PDF
导出
摘要 研究了真空感应熔炼 ( VIM)制备 Cu Cr2 5系触头材料 ,选择水冷凝固及加入 Ni- Al,W- Ni,W- Co二元添加剂得到的触头材料致密度高、氧含量低。讨论了合金元素与微观结构对物理性能与电击穿性能的影响 ,结果表明 ,适当的冷速、合理的添加元素能显著改善材料的显微组织、细化 Cr晶粒 ;W,Co还对 Cr相进行了有效的选择强化 ,合金的耐电压强度明显提高。 The CuCr25 alloys with high density and low oxygen content were prepared by means of vacuum induction melting. The effects of alloying elements (Ni-Al,W-Ni,W-Co) and microstructure on the physical properties and dielectric strength were investigated. The experimental results show that the chromium grains are refined when appropriate solidifying method and alloying elements are selected. On the other hand, the tungsten and cobalt serve the function of strengthening chromium phase. As a result, the dielectric strength increases notably.
机构地区 西安交通大学
出处 《稀有金属材料与工程》 SCIE EI CAS CSCD 北大核心 2001年第4期290-294,共5页 Rare Metal Materials and Engineering
基金 高等学校重点实验室访问学者基金资助
关键词 触头材料 耐电压强度 真空感应熔炼 铜合金 真空断路器 CuCr contact material vacuum induction melting dielectric strength
  • 相关文献

参考文献2

二级参考文献2

共引文献18

同被引文献81

引证文献9

二级引证文献29

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部