摘要 在几个简化假设的前提下 ,采用弹塑性有限元方法 ,系统分析了内压下含轴向裂纹的等径焊制三通的极限载荷及其变化规律 ,分别给出了含轴向裂纹、穿透型裂纹及表面裂纹的三通极限载荷的估算公式 ,并将估算公式计算出的值与有限元数值解进行了比较。结果表明 ,深短裂纹和浅表面裂纹对极限载荷影响很小 ,内表面和外表面两种裂纹形式对极限载荷的影响差别不大 ,可采用外表面裂纹来分析 ; Based on some assumptions, by using the elastic-plastic finite element method, this article studies pressurized equal-diameter welded tee containing axial defects, analyzes systematically the relationship between the limit load and the size of the defects, and presents the estimation methods for the limit load of the tees individually with axial cracks or penetrating cracks or surface cracks. The estimated values of the limit load is compared with the numerical solution of the finite element calculation, and the result shows that, both the deep-short cracks and shallow surface cracks have little effect on the limit load, and the internal surface cracks and the external surface cracks influence the limit load almost to the same degree. The estimation equations presented has high accuracy and reasonable conservative results.
机构地区 华东理工大学
出处 《石油机械》 北大核心 2001年第7期11-14,25,共5页 China Petroleum Machinery
基金 国家"九五"科技攻关项目 (96 -918-0 2 -0 3) 博士点基金资助项目
关键词 等径焊制三通 有限元方法 塑性极限载荷 轴向裂纹 油气输送 equal-diameter welded tee finite element method limit load axial crack
  • 相关文献

参考文献2

二级参考文献7

  • 1沈士明.压力管理的试验与安全评定技术的进展.第一届全国管道学术会议交流会议论文集[M].,1997,7.1-15.
  • 2杜护军.钢制对焊无缝管件和承插焊管件的检验.第一届全国管道学术会议交流会议论文集[M].,1997,7.140-144.
  • 3王有先(译).锅炉和管道钢材及强度计算[M].北京:劳动人事出版社,1983..
  • 4张德姜 等.石油化工装置工艺管道安装设计手册(第1篇),设计与计算[M].北京:中国石化出版社,1992.6.
  • 5-.GB/T9222-88水管锅炉受压元件强度计算[M].北京:国家技术监督局,1989..
  • 6S.S.吉尔.压力容器及其部件的应力分析[M].北京:原子能出版社,1975..
  • 7梅其志,朱卫兵,王昱,张同达,王乃良.受内压焊制三通管件强度的研究[J].压力容器,1992,9(6):20-31. 被引量:6

共引文献16

同被引文献43

引证文献3

二级引证文献2

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部