摘要
Using MgSO4 and NaOH solutions as starting materials, the whisker of 5Mg(OH)2·MgSO4·2H2O has been prepared by hydrothermal method at 160℃ for different time. The whisker was separated, washed by water, ethanol and ether,and characterized by chemical analysis, XRD, IR and microphotography. The growth time of whisker would affect its morphology.
Using MgSO4 and NaOH solutions as starting materials, the whisker of 5Mg(OH)2·MgSO4·2H2O has been prepared by hydrothermal method at 160℃ for different time. The whisker was separated, washed by water, ethanol and ether,and characterized by chemical analysis, XRD, IR and microphotography. The growth time of whisker would affect its morphology.