摘要
铸管公司 3 #高炉大修扩容后 ,通过采取提高精料水平 ,增加风量 ,优化高炉操作 ,加强设备和人员管理等措施 ,使高炉冶炼不断强化 ,2 0 0 0年高炉利用系数达到 3 .48t/ m3.
After overhaul and enlarging the capacity of the No 3 blast furnace, Cast Iron Pipe Corporation adopts the measures of improving level of the beneficiated burden materials, enhancing the amount of air, optimizing the operation of blast furnace and intensifying the management of equipment and personnel, therefore intensify the smelting of blast furnace is constantly intensified The utilization coefficient of blast furnace has reached 3 48t/m\+3 d in 2000
出处
《山东冶金》
CAS
2001年第6期17-19,共3页
Shandong Metallurgy
关键词
高炉
强化冶炼
精料
送风制度
炼铁
blast furnace
intensify smelt
beneficiated burden materials
air blowing system
blast furnace operation