摘要 基于焦散线的形成原理及合裂纹受力试件在裂尖附近区域的应力分布,得到了焦散线法确定应力强度因子的条件:初始曲线半径与试件厚度之比大于0.5。当满足该条件时,对光学各向同性材料及光学各向异性材料前表面反射的情形,只需测量焦散线沿横向的最大尺寸便可较精确地确定应力强度因子;而对于光学各向异性材料的透射或后表面反射情形,只有在忽略远场非奇异应力的影响后,才可借助焦散线的横向尺寸近似确定应力强度因子。 Based on the caustic formation principle and stress distribution near crack tip of loaded specimen, the condition of caustic method for stress intesity factor determination was obtained. The condition is that the proportion of initial curve radius to specimen thickness is larger than 0.5. When the condition is satisfied, the stress intensity factor can be determined by caustic transvers dimension for optically iso-tropic material, as for birefringent material. If the case of front surface reflection is concerned, there is the same conclusion as above. If the case of rear surface reflection or penetration is concerned, the effect of far field nonsingular stress being neglected, the stress intensity factor can be approximately determined by caustic transvers dimension.
出处 《力学季刊》 CSCD 北大核心 2001年第3期359-362,共4页 Chinese Quarterly of Mechanics
关键词 焦散线法 应力强度因子 裂纹受力试件 材料 机械构件 应力场分布 光学各向同性 光学各向异性 裂尖 reflected caustics penetrated caustics optically isotropic optically birefringent stress intensity factor condition
  • 相关文献

参考文献1

二级参考文献1

  • 1张忠平,1990年

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部