摘要
介绍了邯钢400m2烧结机的试生产情况及对工艺参数的测定和优化。针对燃料粒度偏细且配量大、返矿配入量波动、生石灰供应不足、烧结终点控制不当等问题,逐步采取措施进行调整,使烧结工艺参数得到优化,加快了达产速度。
The coarse of trial production and determination and optimization of process parameters of 400m2 sintering machine in Han Steel are introduced. Against the problems: fuel's granularity too small and quantity too large, quantity of return mineral ingredient fluctuant, quick lime not enough, not reasonable end control of sintering etc., various measures were adopted to adjust to optimize the sintering process parameters and speed up the coarse to reach the production target.
出处
《河北冶金》
2002年第1期6-8,共3页
Hebei Metallurgy
关键词
烧结机
工艺参数
优化
试生产
烧结
m2 sintering machine
sintering process parameter
operation of sintering machine