摘要
分析了不锈钢表壳冷挤压模的失效方式 ,采用高强韧性钢 7Cr7Mo2V2Si取代W1 8Cr4V钢 ,并根据表壳模具的特点 ,对 7Cr7Mo2V2Si钢采用合适的锻造与热处理工艺 ,使模具寿命提高 5
The failure forms of cold extrusion mould of stainless steel watch shell are analyzed.By replacing W18Cr4V with 7CrMo2v2Si and adopting properly forging and heat treatment,mould life is improved much more 50 times.