摘要
本文对添加过量TiO_2的BaTiO_3中所形成的第二相Ba_6Ti_(17)O_(40)的动力学进行了高温X射线衍射的实验研究,得到在不同温度下的富钛相Ba_6Ti_(17)O_(40)形成时的反应曲线,计算了反应速率常数K和反应激活能Q,并对第二相形成机制和过量钛的影响进行了讨论。
Kinetics of second phase Ba6Ti17O40 formation in the mixture of BaTiO2 and excess TiO2 were studied by high-temperature X-ray diffraction method. The reaction curves were obtained at various temperatures for the formation of Ti-rich phase Ba6Ti17O40, and the reaction rate constant K and the activation energy Q were calculated. Finally, the mechanism of second phase Ba6Ti17O40 formation and the effect of excess TiO2 are discussed.