研究了原始组织为马氏体、贝氏体和正火态组织的 2 0 Si Mn Ti钢经亚温淬火后的强韧性。结果表明 ,具有马氏体和贝氏体组织的钢 ,经亚温淬火后的强韧性均优于正火态钢。
The strengthening and toughening of 20SiMnTi steel whose original structure are martensite,upper bainite.low bainite and normalized structure respectively and then undergo subcritical quenching have been investigated.The examination results show that after subcrtical quenching the strengthening and toughening of steel with original structure of martensite or bainite is better than that of with normalized one.The effect of strengthening and toughening of steel have much to do with fraction and morphology of two phases
出处
《热加工工艺》
CSCD
北大核心
2002年第3期29-30,共2页
Hot Working Technology
关键词
马氏体
贝氏体
亚温淬火
强韧性
martensite
bainite
subcritical quenching