摘要
以碱渣为主要原料 ,烧制了一种白色水泥 ,通过对不同煅烧温度下所制得水泥性能的测试 ,确定了该水泥的适宜煅烧温度范围为 115 0~ 12 5 0℃。对该适宜煅烧温度下所得的水泥的XRD分析结果表明 ,该水泥的主要矿物为阿利特尼特及少量C1 1 A7·CaCl2 。
A new white cement was burned by soda residue as main raw material. The burning temperature was investigated .The results showed that the optimum burning temperature was in the range of 1 150~1 250℃ by the proper determination of the cement made at various burning temperature .The XRD analytical results showed that the dominate mineral components of the cement are alinite and C 11 A 7·CaCl 2.
出处
《化工矿物与加工》
CAS
北大核心
2002年第6期17-19,共3页
Industrial Minerals & Processing
基金
江苏省教育厅自然科学基金资助项目 (99KJD42 0 0 0 2 )