期刊文献+

超(超)临界锅炉用10Cr18Ni9NbCu3BN钢制管工艺研究 被引量:1

Research on Tube Making Process of 10Cr18Ni9NbCu3BN Steel for USC Boiler
下载PDF
导出
摘要 系统地分析研究了10Cr18Ni9NbCu3BN钢的热穿孔工艺、冷轧工艺、半成品高温软化工艺和成品固溶工艺以及冷轧变形量对成品晶粒度均匀性的影响,重点研究讨论了半成品管不同软化温度和不同保温时间以及成品管不同固溶温度和不同保温时间对成品晶粒度的影响。 In this paper, the effect of hot piercing process, cold rolling process, high temperature softening process of the semi-finished product, solution treatment process of the finished product and cold deformation on the uniformity of the grain size was systematically analyzed. And what' s more, the effect of different softening tem- peratures and hold time as well as different solution treatment temperatures and hold time on the grain size of the finished product was researched.
作者 彭声通
出处 《特钢技术》 CAS 2014年第2期19-24,31,共7页 Special Steel Technology
关键词 10Cr18Ni9NbCu3BN钢 高温软化工艺 成品固溶工艺 晶粒度 10Cr18Ni9NbCu3BN steel, High temperature softening process, Solution treatment process of the finished product, Grain size
  • 相关文献

参考文献3

  • 1哈尔滨锅炉有限责任公司材料研究所编制.四川长城钢管有限公司ASMECODECASE2328-1钢管试验评定报告[Z],2009.03.
  • 2东方锅炉(集团)股份有限公司材料研究所编制.攀钢集团长城特钢有限公司ASTMA-213MS30432不锈钢管评定报告[Z],2009.03.
  • 3科学与技术/中信微合金化技术中心编译.铌[M].北京:冶金工业出版社.2003.08.