摘要 对比了Fe73.5Cu1Mo3Si15.5B7超微晶合金和目前逆变焊机主变压器普遍采用的Fe73.5Cu1Nb3Si15.5B7铁芯的静态和动态磁性能。重点研究了两种材料铁芯的饱和磁致伸缩系数、10-40kHz范围内的高频性能和脉冲性能、-40-140℃间的损耗及磁导率变化。研究结果表明,Fe73.5Cu1Mo3Si15.5B7铁芯可获得低的高频损耗、高磁导率、较低的饱和磁致伸缩系数及良好的温度稳定性,满足逆变焊机主变压器对铁芯材料的要求,同时,Fe73.5Cu1Mo3Si15.5B7带材韧性更高,可改善材料制备的工艺性能和快淬带材的力学性能,提高成材率。 The static and dynamic magnetic properties of cores made of ultrafine crystalline alloy Fe73.5Cu1Mo3Si15.5B7 and Fe73.5Cu1Nb3Si15.5B7 widely used in inverter welder currently were compared.Saturation magnetostriction,performances for high frequency and pulse between 10-40 kHz and the loss and the change of permeability between-40-140℃of the cores were mainly studied.The results show that Fe73.5Cu1Mo3Si15.5B7 core has low high-frequency loss,high permeability,low saturation magnetostriction and excellent temperature stability,which can meet the requirements for transformer of invert welder.Simultaneously,Fe73.5Cu1Mo3Si15.5B7 ribbon has higher toughness,which can improve the process properties and the mechanical properties of ribbon and enhance the yield of core.
出处 《钢铁研究学报》 CAS CSCD 北大核心 2014年第9期53-57,共5页 Journal of Iron and Steel Research
关键词 超微晶合金 热处理工艺 逆变焊机主变压器 高频性能 饱和磁致伸缩系数 温度稳定性 ultrafine crystalline alloy heat treatment process transformer for invert welder high frequency performance saturation magnetostriction temperature stability
  • 相关文献

参考文献10

二级参考文献29

  • 1张小俊.用迈克耳孙干涉仪测量磁致伸缩系数[J].大学物理,1994,13(1):31-31. 被引量:5
  • 2王治,Mater Sci Eng,1997年
  • 3王治,金属学报,1997年,33卷,1289页
  • 4王治,物理学报,1997年,46卷,2054页
  • 5王治,Mater Sci Eng A,1991年,133卷,1页
  • 6纪松,94’秋季中国材料研讨会论文摘要集,1994年
  • 7许裕生,第八届全国磁学磁性材料会议文集,1993年
  • 8张湘义,物理测试,1993年,5卷,203页
  • 9何开元,第六届全国非晶态材料和物理学术讨论会论文集,1991年
  • 10何开元,精密合金材料学,1991年

共引文献24

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部