高含泥氧化铜矿柱浸试验

Column Leaching Test of Copper Oxide with High Content of Clay
下载PDF
导出
摘要 对于某高含泥氧化铜矿,通过不同粒度的水洗矿石做渗透性实验,得出渗透性比较好矿石粒级范围为+2^-25 mm.以此粒度的矿石进行柱浸条件试验,在硫酸浓度60 g/L、液固比2∶1、淋停比2∶1,浸出时间50 d、布液强度为30.0 L/(m2·h)条件下,Fe的浸出率为1.6%左右,吨铜硫酸消耗为14吨左右,铜的浸出率在56%左右. For a sort of copper oxide with high content of clay, by doing permeability experiments with washing ore grainsof different sizes, it is proved that ore grains within the range of +2 - -25 mm are of better permeability. This ore particlesize is thus decided as test condition of column leaching. With the sulfuric acid concentration being 60 g/L, liquid-solidratio 2∶1, leaching-stop ratio 2∶1, leaching time 50 d, liquid fabric strength 30.0 L/(m^2·h), Fe leaching rate is about1.6%, per-ton copper sulphate consumption is about 14 t, and copper leaching rate is about 56%.
作者 赵贺永
出处 《宜宾学院学报》 2014年第12期65-67,共3页 Journal of Yibin University
基金 云南省教育厅科学研究基金项目(2013Y587) 文山学院校级基金项目(13WSY05)
关键词 渗透性 矿石粒度 浸出 permeability ore particle size leaching
  • 相关文献

参考文献5

二级参考文献47

共引文献29

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部