Steel slag carbonation in a flow-through reactor system:The role of fluid-flux 被引量:2

原文传递
导出
摘要 Steel production is currently the largest industrial source of atmospheric CO2. As annual steel production continues to grow, the need for effective methods of reducing its carbon footprint increases correspondingly. The carbonation of the calcium-bearing phases in steel slag generated during basic oxygen furnace(BOF) steel production, in particular its major constituent, larnite {Ca2SiO4}, which is a structural analogue of olivine {(MgFe)2SiO4}, the main mineral subjected to natural carbonation in peridotites, offers the potential to offset some of these emissions. However, the controls on the nature and efficiency of steel slag carbonation are yet to be completely understood. Experiments were conducted exposing steel slag grains to a CO2–H2O mixture in both batch and flow-through reactors to investigate the impact of temperature, fluid flux, and reaction gradient on the dissolution and carbonation of steel slag. The results of these experiments show that dissolution and carbonation of BOF steel slag are more efficient in a flow-through reactor than in the batch reactors used in most previous studies. Moreover, they show that fluid flux needs to be optimized in addition to grain size, pressure, and temperature, in order to maximize the efficiency of carbonation. Based on these results, a two-stage reactor consisting of a high and a low fluid-flux chamber is proposed for CO2 sequestration by steel slag carbonation,allowing dissolution of the slag and precipitation of calcium carbonate to occur within a single flow-through system. Steel production is currently the largest industrial source of atmospheric CO2. As annual steel production continues to grow, the need for effective methods of reducing its carbon footprint increases correspondingly. The carbonation of the calcium-bearing phases in steel slag generated during basic oxygen furnace(BOF) steel production, in particular its major constituent, larnite {Ca2SiO4}, which is a structural analogue of olivine {(MgFe)2SiO4}, the main mineral subjected to natural carbonation in peridotites, offers the potential to offset some of these emissions. However, the controls on the nature and efficiency of steel slag carbonation are yet to be completely understood. Experiments were conducted exposing steel slag grains to a CO2–H2O mixture in both batch and flow-through reactors to investigate the impact of temperature, fluid flux, and reaction gradient on the dissolution and carbonation of steel slag. The results of these experiments show that dissolution and carbonation of BOF steel slag are more efficient in a flow-through reactor than in the batch reactors used in most previous studies. Moreover, they show that fluid flux needs to be optimized in addition to grain size, pressure, and temperature, in order to maximize the efficiency of carbonation. Based on these results, a two-stage reactor consisting of a high and a low fluid-flux chamber is proposed for CO2 sequestration by steel slag carbonation,allowing dissolution of the slag and precipitation of calcium carbonate to occur within a single flow-through system.
出处 《Journal of Environmental Sciences》 SCIE EI CAS CSCD 2015年第1期266-275,共10页 环境科学学报(英文版)
基金 financial support of Tata Steel and NSERC to AEW-J(NSERC-CRD grant number CRDPJ 385478-09)
  • 相关文献

参考文献24

  • 1Bobicki, E.R., Liu, Q.X., Xu, Z.H., Zeng, H.B., 2012. Carbon capture and storage using alkaline industrial wastes. Prog. Energy Combust. Sci. 38 (2), 302-320. http://dx.doi.org/10.1016/j.pecs.2011.11.002.
  • 2Bonenfant, D., Kharoune, L., SauvG S., Hausler, R., Niquette, P., Mimeault, M., et al., 2008. CO2 sequestration potential of steel slags at ambient pressure and temperature. Ind. Eng. Chem. Res. 47 (20), 7610-7616, http://dx.doi.org/lO.lO21/ie701721j.
  • 3Danilov, E.V., 2003. Modern technology for recycling steelmaking slags. Metallurgist 47 (5-6), 232-234.
  • 4Gerdemann, SJ., O'Connor, W.K., Dahlin, D.C., Penner, L.R., Rush, H., 2007. Ex situ aqueous mineral carbonation. Environ. Sci. Technol. 41 (7), 2587-2593. http://dx.doi.org/10.1021/es0619253.
  • 5Huijgen, W.J., Witkamp, G.-J., Comans, R.N., 2005. Mineral CO2 sequestration by steel slag carbonation. Environ. Sci. Technol. 39 (24), 9676-9682. http://dx.doi.orR/10.1021/es050795f.
  • 6International Energy Agency (IEA), 2007. Tracking industrial energy efficiency and CO2 emissions, http://www.iea.org/publications/ freepublications/publication/tracking_emissions.pdf (Paris, France).
  • 7Kelemen, P.B., Matter, J., 2008. In situ carbonation of peridotite for CO2 storage. Proc. Natl. Acad. Sci. U. S. A. 105(45), 17295-17300. http://dx.doi.org/lO.1073/pnas.0805794105.
  • 8Lackner, K.S., Wendt, C.H., Butt, D.P., Joyce, E.L., Sharp, D.H., 1995. Carbon dioxide disposal in carbonate minerals. Energy 20 (11), 1153-1170.
  • 9Lackner, K.S., Butt, D.P., Vendt, C.H., 1997. Progress on binding CO2 in mineral substrates. Energ. Convers. Manage. 38, S259-S264.
  • 10Lasaga, A.C., 1998. Kinetic Theory in the Earth Sciences. Princeton University Press, Princeton.

同被引文献14

引证文献2

二级引证文献11

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部