摘要
采用低温液相催化去钙工艺将含钼40%~41%的钼酸钙转变为氧化钼.结果表明,经处理后的废水钼含量为0.1 g/L以下,生产的氧化钼各项指标达到了工业氧化钼行业标准.
Low temperature liquid phase catalysis process was applied to transform calcium molybdate with 40%-45% calcium into molybdenum oxide. The results show that molybdenum in treated wastewater is 0.1 g/L below, and molybdenum oxide can meet the industrial standard for molybdenum oxide.
出处
《有色金属(冶炼部分)》
CAS
北大核心
2015年第2期39-41,共3页
Nonferrous Metals(Extractive Metallurgy)
关键词
钼酸钙
低温液相
氧化钼
工业氧化钼
calcium molybdate
low temperature liquid
molybdenum oxide
industry molybdenum oxide