摘要 为了综合回收攀枝花低品位钒钛磁铁矿石,对其进行了详细的试验研究。结果表明,采用干式抛尾与阶段磨矿、阶段选别的选矿工艺流程,可获得产率13.65%、TFe品位54.14%、回收率40.56%的合格铁精矿,选铁尾矿采用粗细分选工艺流程可获得产率10.80%、Ti O2品位47.08%、回收率63%的合格钛精矿。 For comprehensive recovery and utilization of low grade vanadium titanium magnetite ore, detailed experimental research were carried out. When using the beneficiation process com-bined with dry discarding of tailings, stage grinding and stage separation, the qualified iron concen-trate with a yield of 13. 65% ,TFe grade of 54. 14% and recovery rate of 40. 56% can be got. The process of coarse and fine separation was used in magnetic separation of rougher tailings, and the eligible titanium concentrate with a yield of 10. 80%, TiO2 grade of 47. 08% and recovery rate of 63% can be obtained.
作者 李林
出处 《矿产保护与利用》 北大核心 2015年第2期27-32,共6页 Conservation and Utilization of Mineral Resources
基金 国家高技术研究发展计划(2012A A062301)
关键词 钛磁铁矿 钛铁矿 磁选 磁滑轮抛尾 粗细分选 titanomagnetite ilmenite magnetic separation tailings discarding by magnetic pul-ley coarse and fine separation
  • 相关文献

参考文献6

二级参考文献6

共引文献44

同被引文献188

引证文献9

二级引证文献29

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部