期刊文献+

板坯角部裂纹控制实践

Practice to Control the Corner Crack of Slab
下载PDF
导出
摘要 分析、讨论了角部表面横裂纹、窄面与宽面角部内裂纹的产生原因,介绍实施的措施及其效果。 The causes of the transversal corner cracks on the slab surface, the inner corner cracks in narrow and wide face were analyzed and discussed; the countermeasures and its effects were introduced .
机构地区 转炉炼钢厂 质量部
出处 《柳钢科技》 2015年第2期7-10,18,共5页
关键词 板坯 连铸 角部表面横裂纹 窄面与宽面角部内裂纹 Slab Continuous Casting Transversal Corner Cracks on the Slab Surface Inner Comer Cracks in the Narrow and Wide face
  • 相关文献

参考文献4

二级参考文献21

  • 1陈小平,杨素波,徐瑜,张龙超.连铸大方坯表面角部纵裂整治实践[J].钢铁,2004,39(z1):240-241. 被引量:3
  • 2赵征志,康永林,于浩,谷海容.CSP工艺生产低碳高强度汽车板力学性能特征及强化机理[J].北京科技大学学报,2005,27(2):227-231. 被引量:4
  • 3刘清友,梁小恺,王雪莲,李德刚,董瀚.薄板坯连铸连轧流程低碳Al镇静钢组织细化原因探讨[J].钢铁,2005,40(8):65-69. 被引量:7
  • 4Akihiko K. Mechanism of the Internal Oxidation Layer Along the Surface Crack on the Slab[J]. TETSU-TO-HAGANE,1995, 81(1):52.
  • 5Akihiko K. Estimation of the Formed Position of the Surface Cracks on the Slab in the Continuous Caster[J]. TETSU-TO-HAGANE, 1996, 82(1):35.
  • 6Upton A. Physical Metallurgy and Mathematical Modeling as Tools for Continuous Casting Optimization at LTV Steel[J].Iron and Steelmaker, 1988, 5:51-57.
  • 7Mintz B. Influence of Composition on the Hot Ductility ofSteels and the Problem of Transverse Cracking[J]. ISIJ International, 1999, 39(9) :833-855.
  • 8Mintz B. Hot-Ductility Behavior of C-Mn-Nb-Al Steels and Its Relationship to Crack Propagation During the Straightening of Continuously Cast Strand[J]. Metals Technology, 1979, (1):24-32.
  • 9Mintz B.Hot Ductility of Directly Cast C-Mn-Nb-Al Steel[J].Material Science and Technology,1986,(2):589.
  • 10Yoshie A.Modeling of Microstructural Evolution and Mechanical Properties of Steel Plates Produced by Thermo-Mechanical Control Process[J].ISIJ International,1992,323:395-404.