针对激光熔覆或3D微打印等金属零件先进制造技术对稳定微量输送金属粉体的要求,分析了微米尺度金属粉体脉冲输送机理。为提高金属粉体脉冲输送分辨率和输送稳定性,设计了余弦修圆波形、正弦修圆波形和正弦余弦组合修圆波形作为压电致动器的驱动电压波形。对平均粒径为100μm的均匀球形TC4钛合金粉体进行了脉冲微输送实验。实验结果表明:余弦修圆波形使粉体做"前进"运动,正弦修圆波形使粉体做"后退"运动;分散态粉体单颗稳定输送达粉体总量的90%,密集态粉体脉冲微输送过程中密实度可控,粉体微输送过程稳定,无结拱现象发生。本文的研究结果也可为其它微米尺度材料或其他形状粉体的脉冲微输送提供参考。
For the requirements of stable micro-feeding of micron metal powder in advanced metal part manufacturing technology including laser cladding and 3D micro-printing, the pulse micro feeding mechanism of micron spherical metal fine powder was researched. To improve the resolution and stability of metal powder micro-feeding, three driving voltage waveforms, including cosine-shape rounded wave, sine shape rounded wave and sine cosine integrated rounded wave, were designed as the driving voltages of the piezoelectric actuator. A pulse micro-feeding experiment for the uniform spherical TC4 titanium alloy powder with an average diameter of 100μm was performed. The experiment result show that the cosine-shape rounded wave makes the powder go forward while the sine shape rounded wave makes the powder go back. The percentage of the dispersing state powder transported one by one has reached 90%. The powder degree of compaction can be controlled. The powder micro-feeding process is stable obtained results provide references for materials and different shapes. without the phenomenon of the micro-feeding of other powder arch accumulation. The kinds of powder with different
出处
《光学精密工程》
EI
CAS
CSCD
北大核心
2015年第6期1620-1626,共7页
Optics and Precision Engineering
基金
中国博士后科学基金资助项目(No.2014M551584)
江苏省博士后科研基金资助项目(No.1402006B)
江苏省三维打印装备与制造重点实验室开放基金资助项目(No.L2014071302)
关键词
激光熔覆
金属微粉体
微输送
脉冲惯性力
微喷嘴
laser cladding deposition
metal fine powder
micro-feeding
pulse inertia force
micro-nozzle