摘要
研究了预先退火温度和保温时间对2A96铝锂合金的力学性能和组织的影响,确定了该合金的预先退火工艺为460℃/2h,在工业化生产中已经得到了应用。
Effect of pre-annealing temperature and holding time on microstructure and property of 2A96 Al-Li alloy was researched. It is confirmed that the pre-annealing process is 460℃/2h, which is applied in industrial production.
出处
《铝加工》
CAS
2015年第3期35-37,共3页
Aluminium Fabrication
关键词
再结晶
晶粒粗大
预先退火
加工硬化
recrystalization
grain coarsening
pre-annealing
work-hardening