摘要 采用对比的方式,分别对天然蛇纹石和经700%改性的蛇纹石做了等温吸附实验,研究蛇纹石对重金属Cd2’的吸附性能,并探讨了影响吸附的因素和吸附机理。吸附剂用量、溶液的pH值对2种蛇纹石的吸附率均有较大影响。随着吸附剂用量的增加,天然蛇纹石和热改性蛇纹石对cd2+的吸附率都逐渐增加,且吸附率都超过了60%。在同等吸附剂用量条件下,经7000C改性的蛇纹石的吸附能力要明显强于未改性的天然蛇纹石。当pH值为3—6时,2种蛇纹石对Cd2+的吸附量都随着pH值的增加而显著增大;当pH值为6~10时.对cd2+的吸附量趋于稳定。两种蛇纹石均符合Freundlich方程,且拟合度较好,对重金属cd2+有较强的吸附能力;经700℃改性的蛇纹石对cd2+的饱和吸附量为8.19mg/g,约等于天然蛇纹石饱和吸附量的2倍。 An isothermal adsorption test was made between natural serpentine and thermal-modified serpentine at 700℃ to remove the heavy ion Cd2+. This paper discusses the factors and mechanism of adsorption. Adsorption ratio depends largely on adsorbent quantity and solution pH value. Adsorption ratio rises up to over 60% with more adsorbent. Thermal-modified serpentine is obviously better than natural serpentine in adsorption ability with the same amount of adsorbent. The adsorption capacity of both increases as pH value rises from 3 to 6, and tends to be stabilized as pH value is 6 - 10. Two kinds of serpentine are in accordance with Freundlich formula with a good fitting. The maximum adsorption quantity of thermal-modified serpentine at 700℃ is 8. 19 mg/g, approximately twice that of the natural serpentine.
出处 《资源与产业》 2015年第4期56-60,共5页 Resources & Industries
关键词 天然蛇纹石 热改性蛇纹石 除镉 吸附量 natural serpentine thermal-modified serpentine cadmium adsorption adsorption quantity
  • 相关文献

参考文献17

二级参考文献166

共引文献151

同被引文献66

引证文献3

二级引证文献11

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部