摘要
重钢二炼钢厂通过对转炉出钢合金化、LF炉升温造渣、LF炉合金化、LF炉吹氩等工艺的改进优化,使LF炉精炼结束后钢水[C]元素成份命中率大幅提高,品种炼成率稳定在98%以上。
After a series of improving measures of LF furnace in No.2 steel plant Chongqing Steel such as the converter steel alloying, temperature of slag, alloying and argon blowing process in LF furnace. The [C] element hit ratio raised significantly after LF furnace refining the rate of finished products up to 98%.