摘要 采用超声波细胞破碎机和激光粒度仪等仪器设备进行了煤油乳化试验,探究不同乳化条件与乳化煤油粒度的关系。研究发现,当超声细胞粉碎机输出功率为60%,超声时间为2 min时,乳化煤油的粒度随着乳化剂添加量的增加而减小。隐晶质石墨浮选试验结果表明:乳化煤油粒度越小,越有利于乳化液在细粒石墨表面附着,浮选效果越好。 Ultrasonic processor and laser particle size analyzers were used to perform the kerosene emulsion tests, to explore the relationship between different emulsifying conditions and granularity of the emulsiifed kerosene. It was found that the granularity of emulsiifed kerosene was decreased with the increase of the added dosage of emulsiifer X-100 with the output power of ultrasonic processor was 60% and the emulsifying time was 2 min. The lfotation results of amorphous graphite indicated that the smaller the particle size of the emulsiifed kerosene, the easier to adhere on the surface of the ifne graphite, and the lfotation effect was better.
出处 《非金属矿》 CAS CSCD 北大核心 2015年第5期48-49,53,共3页 Non-Metallic Mines
关键词 乳化煤油 乳化剂 粒度 隐晶质石墨 浮选 emulsiifed kerosene emulsiifer particle size amorphous graphite lfotation
  • 相关文献

参考文献7

二级参考文献10

  • 1卢文光,王祖讷.一种选别隐晶质石墨的新方法[J].非金属矿,1994,17(1):17-18. 被引量:6
  • 2格列姆博茨基.浮选过程物理化学基础[M].北京:冶金工业出版社,1985..
  • 3中国金属学会选矿学术委员会.选矿技术[M].中国选矿科技情报网,1984,127.
  • 4斯坎伦 M J,国外金属矿选矿,1993年,8期,3页
  • 5Shirley C Tsai. Effects of Surface chemistry and particle size and density on froth flotation of fine coal [J]. Colloids and Surfaces, 1985, 16:323 -336.
  • 6Z Aktas, E T Woodburn. The effect of non - ionic reagent absorption on the froth structure and flotation performance of two low rank British coals [J] . Power Technology, 1995, 83: 149-158.
  • 7毛培坤.表面活性剂产品工业分析[M].北京:化学工业出版社,2002..
  • 8徐淘.隐晶质石墨选择性絮凝分选初探[J]非金属矿,1988(01).
  • 9王斌,陈忠典.推广先进技术 提高技术经济指标[J].中国钼业,2000,24(2):29-31. 被引量:2
  • 10吉根朝.隐晶质石墨浮选中间试验研究[J].非金属矿,1991(2):16-18. 被引量:6

共引文献36

同被引文献101

引证文献8

二级引证文献30

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部